New Publication about carbon steel and pitting corrosion in Corrosion Science

A new article detailing the “Long-term survival of Desulfovibrio vulgaris on carbon steel and associated pitting corrosion” has been published in Corrosion Science by Yajie Chen, Qiong Tang, John M. Senko, Gang Cheng, Bi-min Zhang Newby, Homero Castaneda, Lu-Kwang Ju.